Patterns created by the superimposition of two or more light-colored screens in printing, exhibiting intermittent instances of dot-free transfer, resembling the night sky with scattered stars. Here and there, you may notice a few white dots, often appearing as small circular areas lacking ink. This phenomenon is distinct from ink shortage or plate blockage. Consider a bowl produced by overlaying blue and red light-colored screens. If you observe star-like white dots on the bowl's surface, careful observation will reveal whether these dots exhibit a blue or red cast. If it's a blue cast, it indicates a red dot, and vice versa.

High viscosity of an unrelated but large-area color (less common)

Decrease the viscosity of the preceding color (e.g., if reducing the viscosity of red ink doesn't work in the case of red-blue overprinting, consider reducing the viscosity of blue ink)

Reduce the viscosity of the preceding unrelated but large-area color (e.g., in the case of Kangshifu's classic condensed milk-flavored milk tea with blue-red-yellow overlapping, if blue and red dots appear, and the base color (first color pearlescent white) is hollow in the pattern area, lowering the viscosity of the base color to Less than or equal to 12.0 seconds immediately improves dot retention.)

Poor adhesion between ink and the original film, where ink can be easily scraped off or detached. A common inspection method is to use 3M tape to adhere to the printed ink surface, then peel off the tape at a speed of 1m/second. Generally, if 90% of the ink does not come off, it is considered acceptable. Transparent tape is often used during printing for a simple adhesion test because it has a stronger adhesive force than 3M tape and is more cost-effective.

Sende bookingforespørsel

whatsapp

Telefon

E-post

Forespørsel